Question
Offered Price $5.00

A turbine disk made from a Ni-base superalloy

Question # 00157421
Subject: Engineering
Due on: 01/22/2016
Posted On: 12/23/2015 01:45 AM
Expert tutors with experiences and qualities
Posted By
kimwood
Best Tutors for school students, college students
Questions:
114006
Tutorials:
113886
Feedback Score:

Purchase it
Report this Question as Inappropriate
Question

A turbine disk made from a Ni-base superalloy will be operating at

1350F. The creep data are given below. Determine the maximum stress allowable if

the design criterion requires less than 1% strain in 10,000 hours.

Tutorials for this Question
Available for
$5.00

A turbine disk made from a Ni-base superalloy

Tutorial # 00151964
Posted On: 12/23/2015 01:45 AM
Posted By:
Best Tutors for school students, college students kimwood
Expert tutors with experiences and qualities
Questions:
114006
Tutorials:
113886
Feedback Score:
Report this Tutorial as Inappropriate
Tutorial Preview …data xxx given xxxxx Determine the…
Attachments
soln-new.zip (216.76 KB)
Preview not available.
Purchase this Tutorial @ $5.00 *
* - Additional Paypal / Transaction Handling Fee (3.9% of Tutorial price + $0.30) applicable